MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Indium Corp. 3N Commercial Indium Metal
Categories: Metal; Nonferrous Metal; Indium Alloy; Pure Element

Material Notes: Indium is a versatile metal with unique physical properties.
  • Indium has one of the widest liquid temperature ranges of any metal.
  • Indium has a low vapor pressure, making it ideal for high vacuum applications.
  • Indium is a soft, pliable and malleable, even down to cryogenic temperatures
  • Relatively low toxicity
  • Indium is a bright shiny metal that forms a thin (80 - 100 angstroms) protective oxide layer. It is used as a decorative trim coating metallization on plastics for appliance and automobile trim.
  • Indium effectively reduces the melting point in solder alloys and fusible alloys.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.30 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 157 °C
Boiling Point 2080 °C
 
Component Elements PropertiesOriginal ValueComments
Bismuth, Bi 0.0060 %
Cadmium, Cd 0.0060 %
Copper, Cu 0.0042 %
Indium, In 99.9 %
Iron, Fe 0.00030 %
Lead, Pb 0.0086 %
Nickel, Ni 0.00050 %
Silver, Ag 0.00010 %
Thallium, Tl 0.00020 %
Tin, Sn 0.0185 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Indium Alloy
In90-Ag10 Indium-Silver Solder
In97-3Ag Indium-Silver Solder
AIM 97In/3Ag Solder for Photonic Packaging
AIM 47 Fusible Bismuth Alloy

NNIN910 / 131549

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.