MVR (300 °C/1.2 kg) 13 cm³/10 min; LED Lighting, optics and lenses; PC with highest transmission; medium viscosity; UV stabilized; injection molding - melt temperature 280 - 320 °C; available in color code 551053 onlyAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |