MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Molded

Material Notes: Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most dimensionally stable thermoplastics available. It is used for a variety of structural applications including electrical housings, scientific instrumentation parts, and fluid handling components.

Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
Water Absorption 0.070 %ASTM D570; 24 hrs.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D7852
Tensile Strength, Yield 9200 psiASTM D638
Elongation at Break 25 %ASTM D638
Flexural Yield Strength 14400 psiASTM D790
Flexural Modulus 370000 psiASTM D790
Izod Impact, Notched 3.50 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.69
@Frequency 60 Hz
ASTM D150
Dielectric Strength 50.0 kV/mmASTM D149
Dissipation Factor 0.00070
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 254 °FASTM D648
Flammability, UL94 V-1
@Thickness 1.47 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1799 X 138211 C Modified Polyphenylene Oxide (PPO); Glass Fiber - Flame Retardant
RTP Company RTP 1701 Modified Polyphenylene Oxide (PPO), Glass Fiber
LNP Lubriloy® Z- BK8-950 Polyphenylene Ether + Polystyrene, Proprietary Filler
EPICHEM Epiryl PPO V0 Polyphenylene oxide
EPICHEM Epiryl B PPO Polyphenylene oxide

PWEST004 / 72708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.