MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems Accura® Xtreme Plastic for SLA® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: For use with solid-state stereolithography (SLA®) systems

    Applications
  • Form, fit and function prototypes
  • Durable Assemblies
    • Snap fit assemblies
    • Tough enclosures
    • Consumer electronic components
  • Master patterns for RTV/Silicone molding
  • Replace CNC machining of Polypropylene and ABS

    Features
  • Look and feel of a durable molded plastic
  • Outstanding durability and impact resistance
  • Thermal Resistance over 60° C
  • Easy to use low viscosity formulation
  • Fully developed and tested build styles
  • All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. Leaders in producing fast Rapid Manufacturing and Prototyping solutions using the major 3D printing systems including SLA printing technology. Free 3D printing quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
@Temperature 28.0 °C
Liquid
 1.19 g/cc
@Temperature 25.0 °C
Solid
Viscosity 250 - 300 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 38.0 - 44.0 MPaASTM D638
Elongation at Break 14 - 22 %ASTM D638
Tensile Modulus 1790 - 1980 MPaASTM D638
Flexural Strength 57.0 - 71.0 MPaASTM D790
Flexural Modulus 1520 - 2070 MPaASTM D790
Izod Impact, Notched 35.0 - 52.0 J/mASTM D256
Penetration 4.1mils
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °CASTM D648
Glass Transition Temp, Tg 70.0 - 74.0 °CDMA, E"
 
Descriptive Properties
AppearanceGrey
Critical Exposure (mJ/cm²)11.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3D Systems Accura® Xtreme White 200 Plastic
ALM D80-ST Nylon 11 SLS Prototyping Polymer
3D Systems Accura® 10 Plastic for SLA® Systems
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Tipco Tipcofil® KMX 800 FR - UL94-V0 Flame Retardant, Highly Filled PBT/PC Alloy, with High Heat Stability

PAPPR101 / 83480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.