MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene® LD-401 EVA for Electrical Insulation  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.

Applications: Base resin for fully formulated low voltage cable insulations compounds.

Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.927 g/ccExxon Method
Environmental Stress Crack Resistance >= 1000 hourF50, Condition A; ASTM D1693
Melt Flow 3.6 g/10 minExxon Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40ASTM D2240
Tensile Strength, Ultimate 11.7 MPaASTM D638
Elongation at Break 750 %ASTM D638
Flexural Modulus 0.0830 GPaASTM D790
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.45
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.3 kV/mm
@Thickness 3.17 mm
ASTM D149
Dissipation Factor 0.0080
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 96.0 °CExxon Method
Brittleness Temperature <= -72.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil EVA 14018.07 Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
ExxonMobil Escorene™ Ultra UL 7765 Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
ExxonMobil Escorene™ Ultra LD 783 CD Ethylene Vinyl Acetate Copolymer (EVA)
ExxonMobil Escorene® UL-7560 EVA Copolymer, Adhesive and Sealant Grade
ExxonMobil Escorene® UL 7765 Adhesive Application Resin

PEXCHL / 38005

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.