MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ampco Metal AMPCO® 8 Aluminum Bronze, Extruded and Drawn Rods, 12.7 - 25.4 mm.
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: AMPCO 8 extruded has a high tensile strength and a good yield along with an inherent toughness and ductility not usually found in a single alpha phase aluminum bronze. During the extrusion process the metal is hot worked resulting in a compact grain structure free of inclusions or other defects and improved physical properties.

Applications: AMPCO 8 is used whenever good resistance to corrosion, erosion, abrasion and cavitation-pitting is essential. AMPCO 8 is ideally suited for pipes, tubes, joints and other pieces used in the process, marine or other similar industries. The extreme hardness of this alloy makes it an ideal bolting material. AMPCO 8 has excellent bearing characteristics. It is used for bushings, bearings, wear strips and in similar applications where hardness and ductility are essential for uninterrupted operations.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.95 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 183HB 30
Hardness, Rockwell B 90
Tensile Strength, Ultimate 565 MPa
Tensile Strength, Yield 358 MPa
@Strain 0.5 %
Elongation at Break 35 %
Reduction of Area 55 %
Modulus of Elasticity 124 GPa
Compressive Yield Strength 165 MPaProportional Limit
 324 MPa0.1% Perm. Set
Compressive Strength 896 MPa
Shear Strength 310 MPa
Izod Impact 68.0 J
Charpy Impact 47.0 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000142 ohm-cm12% I.A.C.S.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.3 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 54.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 6.5 %
Copper, Cu 90.25 - 90.75 %As Balance
Iron, Fe 2.5 %
Other, total <= 0.50 %
Tin, Sn 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum bronze 5%, UNS C60800
Ampco Metal AMPCO® 21 Aluminum Bronze, Rectangular
Ampco Metal AMPCO® 8 Aluminum Bronze, Extruded and Drawn Rods, 50.8 - 76.2 mm.
Ampco Metal AMPCO® 45 Nickel-Aluminum Bronze, Extruded and Drawn Rods, ≤ 25.4 mm.
International Mold Steel Daido DRM1 Matrix High-Speed Steel

NAMPCO01 / 14955

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.