MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Starex® SD-0150UF ABS, Unreinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes:

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Melt Flow 11 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103ASTM D785
Tensile Strength at Break 31.4 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 400 kg(f)/cm²5 mm/min; ASTM D638
Elongation at Break 16 %5 mm/min; ASTM D638
Tensile Modulus 20000 kg(f)/cm²5 mm/min; ASTM D638
Flexural Strength 58.8 MPa2.8 mm/min; ASTM D790
Flexural Modulus 20000 kg(f)/cm²2.8 mm/min; ASTM D790
Izod Impact, Notched 29.0 kg-cm/cm
@Thickness 6.35 mm
ASTM D256
 36.0 kg-cm/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point 96.0 °CB/50; ISO R306
 99.0 °CB/120; ISO R306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tabriz SD-0150 General Purpose ABS
LG Chemical RX710 ABS, High Impact, Chemical Resistance to HCFC
Stratasys® ABS-M30
Techmer ES Plastiblend® ABS 8003 A1
Lotte Advanced Materials Starex® SP-0183 ABS, Unreinforced Extrusion Grade

PSAMSU858 / 146675

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.