MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Dehesive® EM 426 Silicone Release Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: DEHESIVE® EM 426 is the base polymer to a three component aqueous emulsion system. It is used in combination with WACKER® CROSSLINKER V 15 and WACKER® CATALYST EM 454. The product is designed for pressure sensitive adhesive release applications and works on papers of varying porosity and films. Cure is achieved using a vinyl addition chemistry mechanism.

Special features:

  • Good anchorage on a wide variety of paper substrates
  • Formulation flexibility allows for variation of hydrogen: vinyl (SiH:SiVi) mole ratio and platinum catalyst content
  • Compatibility with various thickening agents allows for absorbent substrate processing
  • Adjustable release level when used in conjunction with CRA® EM 456

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccDIN 51757
Solids Content 54 %
Viscosity 500 cPdynamic
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Dehesive® 919 Silicone Release Coating
Wacker Dehesive® 944 Silicone Release Coating
Wacker Dehesive® SFX 251 AMA® Silicone Release Coating
Wacker Dehesive® SFX 250 Silicone Release Coating
Wacker Dehesive® SF 500 Silicone Release Coating

PWACK9072 / 204601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.