MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec Sikor® S Cordierite
Categories: Ceramic; Oxide; Aluminum Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as cost-effective extruded and dry-pressed forms. Sikor® S offers higher compressive strength with slightly lower thermal shock resistance than other cordierites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.20 g/ccDIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %DIN EN 623-2 / ASTM-C373
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 70.0 GPaYoung's; DINV ENV 843-2 / ASTM-F417
Compressive Strength 500 MPaASTM C-773-88 / DIN 51067T1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1e+05
@Temperature 500 °C
 1.00e+12 ohm-cm
@Temperature 100 °C
IEC 672-1
Dielectric Constant 5.0
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Loss Index 0.0070
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-D149,150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.00 µm/m-°C
@Temperature 20.0 - 200 °C
 2.00 - 3.00 µm/m-°C
@Temperature 20.0 - 600 °C
ASTM-C373
 2.00 - 4.00 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.900 J/g-°C
@Temperature 100 - 200 °C
DINV ENV 821-3
Thermal Conductivity 2.20 W/m-KDIN EN 821-2 / ASTM-C408
 
Descriptive Properties
ColorBrown
Thermal Shock Resistance R1 (K)250Hasselman (Experimental)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning ULE® 7972 Ultra Low Expansion Glass
CeramTec Sikor® E Cordierite
Aluminum 6082-T6
Aluminum 6063-T5
Schott ZERODUR® Glass Ceramic

CCERA927 / 107527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.