MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
C.O.I.M. LARIPUR® LPR2102-85AE Polycaprolactone Ester Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:
  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Series 2102 Polycaprolactone Ester: Products based on polycaprolactones; they have the same features as TPU based on quality ester. Compared with series 25, they show a higher resistance to hydrolysis and very good elastic memory.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 84ASTM D2240
Tensile Strength, Yield 65.0 MPaASTM D412
Elongation at Break 510 %ASTM D412
50% Modulus 0.00430 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.00620 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0175 GPa
@Strain 300 %
ASTM D412
Tear Strength 72.0 kN/mASTM D624
Abrasion 30mm3, Abrasion Loss; DIN 53516
Compression Set 36 %
@Temperature 70.0 °C
Method B, 22 hours; ASTM D395
 17 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 89.0 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane
Elastomer Engineering E850-85A Polyurethane
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer

PCOIM015 / 28618

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.