MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 5454-H34
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95454; ISO AlMg3Mn; Aluminium 5454-H34; AA5454-H34; Al5454-H34
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.69 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 81AA; Typical; 500 g load; 10 mm ball
Tensile Strength, Ultimate 44.0 ksiAA; Typical
 41.0 MPa
@Temperature 371 °C
 75.0 MPa
@Temperature 316 °C
 115 MPa
@Temperature 260 °C
 180 MPa
@Temperature 204 °C
 235 MPa
@Temperature 149 °C
 295 MPa
@Temperature 100 °C
 305 MPa
@Temperature -28.0 °C
 305 MPa
@Temperature 24.0 °C
 315 MPa
@Temperature -80.0 °C
 435 MPa
@Temperature -196 °C
Tensile Strength, Yield 35.0 ksiAA; Typical
 29.0 MPa
@Temperature 371 °C
 50.0 MPa
@Temperature 316 °C
 75.0 MPa
@Temperature 260 °C
 130 MPa
@Temperature 204 °C
 195 MPa
@Temperature 149 °C
 235 MPa
@Temperature 100 °C
 240 MPa
@Temperature -28.0 °C
 240 MPa
@Temperature 24.0 °C
 250 MPa
@Temperature -80.0 °C
 285 MPa
@Temperature -196 °C
Elongation at Break 16 %
@Temperature 24.0 °C
 18 %
@Temperature -28.0 °C
 18 %
@Temperature 100 °C
 21 %
@Temperature -80.0 °C
 30 %
@Temperature -196 °C
 32 %
@Temperature 149 °C
 45 %
@Temperature 204 °C
 80 %
@Temperature 260 °C
 110 %
@Temperature 316 °C
 130 %
@Temperature 371 °C
 10 %
@Thickness 1.59 mm
AA; Typical
Modulus of Elasticity 10200 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Notched Tensile Strength 310 MPa2.5 cm width x 0.16 cm thick side-notched specimen, Kt = 17.
Ultimate Bearing Strength 538 MPaEdge distance/pin diameter = 2.0
Bearing Yield Strength 338 MPaEdge distance/pin diameter = 2.0
Poissons Ratio 0.33Estimated from trends in similar Al alloys.
Fatigue Strength 125 MPa
@# of Cycles 5.00e+8
unnotched R. R. Moore rotating beam
Shear Modulus 26.0 GPaEstimated from similar Al alloys.
Shear Strength 26.0 ksiAA; Typical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000510 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.1 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical; average over range
 21.9 µm/m-°C
@Temperature -50.0 - 20.0 °C
 23.7 µm/m-°C
@Temperature 20.0 - 100 °C
 24.6 µm/m-°C
@Temperature 20.0 - 200 °C
 25.6 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.900 J/g-°C
Thermal Conductivity 134 W/m-K
Melting Point 1115 - 1195 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 1115 °FAA; Typical
Liquidus 1195 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 650 °Fholding at temperature not required
Hot-Working Temperature 500 - 950 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 94.4 - 97.1 %As remainder
Chromium, Cr 0.05 - 0.20 %
Copper, Cu <= 0.10 %
Iron, Fe <= 0.40 %
Magnesium, Mg 2.4 - 3.0 %
Manganese, Mn 0.50 - 1.0 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.25 %
Titanium, Ti <= 0.20 %
Zinc, Zn <= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6061-T8
Aluminum 5454-H32
Aluminum 2124-T351
Aluminum 7075-T6; 7075-T651
Aluminum 1050-H14

MA5454H34 / 9279

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.