MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nanocyl PREGCYL™ NC R2HM-01 Pre-impregnated UD/Fabric Carbon Fibers
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: PREGCYL™ NC R2HM-01 is a pre-impregnated material based on our EPOCYL NC R2HM01 formulated epoxy resin system modified with our own Carbon Nanotubes (CNT) and specifically developed to enhance the mechanical properties of the final composite parts.

Applications: High performance composite parts

  • Automotive (bumpers and other structural parts)
  • Marine, especially sailing boats (structural outer shell in carbon fiber composite, masts and other generic structural parts)
  • Industrial parts (rollers, doctor-blades and wind-mill blades)
  • Sporting equipments (bike frames, hockey sticks, tennis rackets, skis and golf shafts)
  • Aerospace (structural parts and interiors)

Advantages High toughness (over 1200j/m2 in some configurations), Low CTE, 120 degrees C Tg, Easy and ready to use, Higher uniformity of temperature during curing (avoids hot-spots)

Examples of fibers and fabrics available

  • 200 g/m² plain and twill 2/2 weave, 3K; 45% resin content
  • 370 g/m² Harness 5 weave, 6K; 45% resin content
  • 400 g/m² twill 2/2 weave, 12K; 45% resin content
  • 600 g/m² twill 2/2 weave, 12K; 45% resin content
  • 150 g/m² UD; 37% resin content
  • 100 g/m² UD; 37% resin content

Properties of the cured and fiber reinforced composite The values given are for pressed laminates comprising 8 layers of unidirectional (UD) carbon fibers high tenacity (Tenax 12K HTS 5631) fo 230 g/m². Fiber volume fraction: 58-60%. Curing cycle: 1h at 120°C + 2h at 140°C combined with low pressure.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 553 MPaASTM D3410
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4000 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 29.7 µm/m-°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC
Overview of materials for Epoxy/Carbon Fiber Composite
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System
Overview of materials for Epoxy Adhesive
Overview of materials for Epoxy Adhesive, Flexible

ENANOC959 / 108954

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.