MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical XG568 MABS, Anti-Scratch, High Gloss
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Feature: Injection Molding, Anti-Scratch, High Gloss

Application: LCD TV Front Cabinet, Bezel, Audio/Video Housing

CSA No. 9011-14-7 and 9003-56-9

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
0.30 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Maximum Moisture Content 0.0100.010Injection Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 19.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
19.5 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ASTM D785
Tensile Strength, Yield 53.0 MPa
@Thickness 3.20 mm
7680 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 20 %
@Thickness 3.20 mm
20 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Yield >= 6.0 %
@Thickness 3.20 mm
>= 6.0 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Yield Strength 85.3 MPa
@Thickness 3.20 mm
12400 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 2.75 GPa
@Thickness 3.20 mm
398 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  0.883 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
1.65 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 0.883 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.65 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  0.392 J/cm
@Thickness 6.40 mm,
Temperature -20.0 °C
0.735 ft-lb/in
@Thickness 0.252 in,
Temperature -4.00 °F
ASTM D256
 0.392 J/cm
@Thickness 3.20 mm,
Temperature -20.0 °C
0.735 ft-lb/in
@Thickness 0.126 in,
Temperature -4.00 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi)  86.0 °C
@Thickness 3.20 mm
187 °F
@Thickness 0.126 in
ASTM D648
 88.0 °C
@Thickness 6.40 mm
190 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  82.0 °C
@Thickness 3.20 mm
180 °F
@Thickness 0.126 in
ASTM D648
 83.0 °C
@Thickness 6.40 mm
181 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Flammability, UL94  HB
@Thickness >=1.60 mm
HB
@Thickness >=0.0630 in
 HB
@Thickness >=3.20 mm
HB
@Thickness >=0.126 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 200 °C356 - 392 °FInjection Molding
Middle Barrel Temperature 190 - 210 °C374 - 410 °FInjection Molding
Front Barrel Temperature 200 - 220 °C392 - 428 °FInjection Molding
Nozzle Temperature 200 - 220 °C392 - 428 °FInjection Molding
Melt Temperature 200 - 230 °C392 - 446 °FInjection Molding
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection Molding
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPa4260 - 8530 psiInjection Molding
Screw Speed 30 - 60 rpm30 - 60 rpmInjection Molding
 
Descriptive Properties
Ozone ResistanceNo Crack5 sec, JIS K6301

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical HF350U ABS, High Flow
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus
LG Chemical LUCEL VC127-LD Antistatic POM, Unreinforced, High Flow, For VCR Reels
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled
LG Chemical HI100K ABS, High Impact

PLAY030 / 148038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.