System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LG Chemical XG568 MABS, Anti-Scratch, High Gloss
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Molded
Material Notes:
Feature: Injection Molding, Anti-Scratch, High Gloss
Application: LCD TV Front Cabinet, Bezel, Audio/Video Housing
CSA No. 9011-14-7 and 9003-56-9
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.11
g/cc
ASTM D792
Water Absorption
0.30 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Maximum Moisture Content
0.010
Injection Molding
Linear Mold Shrinkage, Flow
0.0020
-
0.0040
cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow
19.5
g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
114
ASTM D785
Tensile Strength, Yield
540
kg(f)/cm²
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Break
20 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Yield
>= 6.0 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Flexural Yield Strength
870
kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Flexural Modulus
28000
kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Izod Impact, Notched
9.00
kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
9.00
kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched
4.00
kg-cm/cm
@Thickness 6.40 mm,
Temperature -20.0 °C
ASTM D256
4.00
kg-cm/cm
@Thickness 3.20 mm,
Temperature -20.0 °C
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
86.0
°C
@Thickness 3.20 mm
ASTM D648
88.0
°C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
82.0
°C
@Thickness 3.20 mm
ASTM D648
83.0
°C
@Thickness 6.40 mm
Unannealed; ASTM D648
Flammability, UL94
HB
@Thickness >=1.60 mm
HB
@Thickness >=3.20 mm
Processing Properties
Original Value
Comments
Rear Barrel Temperature
180
-
200
°C
Injection Molding
Middle Barrel Temperature
190
-
210
°C
Injection Molding
Front Barrel Temperature
200
-
220
°C
Injection Molding
Nozzle Temperature
200
-
220
°C
Injection Molding
Melt Temperature
200
-
230
°C
Injection Molding
Mold Temperature
40.0
-
60.0
°C
Injection Molding
Drying Temperature
80.0
-
90.0
°C
Injection Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
Back Pressure
29.4
-
58.8
MPa
Injection Molding
Screw Speed
30
-
60
rpm
Injection Molding
Descriptive Properties
Ozone Resistance
No Crack
5 sec, JIS K6301
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
LG Chemical HF350U ABS, High Flow
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus
LG Chemical LUCEL VC127-LD Antistatic POM, Unreinforced, High Flow, For VCR Reels
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled
LG Chemical HI100K ABS, High Impact
PLAY030 / 148038
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.