MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Kynar Flex® 2821-00 Polyvinylidene Fluoride Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purity

Applications:

  • Chemical processing – production, storage and transfer of corrosive fluids
  • Electronics – protective sheathing, plenum and wiring insulation
  • Semi-conductor industry
  • Food stuff and Healthcare industries
  • Transportation – fuel line and pipe, thermoformed body components

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.77 - 1.80 g/ccASTM D792
Density 1.77 g/ccISO 1183
Water Absorption 0.030 %Dry; Sim. to ISO 62
Viscosity 1.20e+6 - 2.00e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
Melt; ASTM D3835
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
cm³/10 min Volumetric Rate; ISO 1133
 1.0 - 8.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60 - 70ASTM D2240
Tensile Strength at Break 17.2 - 34.5 MPaASTM D638
Tensile Strength, Yield 27.0 MPaDry; ISO 527-1/-2
 20.0 - 34.5 MPaASTM D638
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 100 - 300 %ASTM D638
Elongation at Yield 15 %Dry; ISO 527-1/-2
Tensile Modulus 700 MPaDry; ISO 527-1/-2
 552 - 896 MPaASTM D638
Flexural Modulus 483 - 758 MPaASTM D790
Compressive Strength 31.0 - 41.4 MPaASTM D695
Izod Impact, Notched 534 - 1070 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
Charpy Impact, Notched NB
@Temperature 23.0 °C
Dry; ISO 179/1eA
Coefficient of Friction, Dynamic 0.33vs. steel; ASTM D1894
Coefficient of Friction, Static 0.33vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 9.0 - 16CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cm65% R.H; ASTM D257
 2.00e+14 ohm-cmDry; IEC 60093
Dielectric Constant 6.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 3.5 - 10.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 1.30 - 1.50 kV/mmASTM D149
Dissipation Factor 0.057
@Frequency 100 Hz
Dry; IEC 60250
 0.020 - 0.21
@Frequency 100000 Hz
ASTM D150
 0.234
@Frequency 1e+6 Hz
Dry; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 126 - 185 µm/m-°CASTM D696
CTE, linear, Parallel to Flow 160 µm/m-°CDry; ISO 11359-1/-2
Specific Heat Capacity 0.745 - 0.958 J/g-°CDSC
Thermal Conductivity 0.144 - 0.180 W/m-KASTM D433
Melting Point 140 - 145 °CASTM D3418
 143 °C10°C/min; Dry; ISO 11357-1/-3
Maximum Service Temperature, Air 130 °CUL RTI
Deflection Temperature at 0.46 MPa (66 psi) 60.0 - 75.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 55.0 °CASTM D648
 48.0 °CDry; ISO 75-1/-2
Vicat Softening Point 76.0 °C50°C/h 50N; Dry; ISO 306
Glass Transition Temp, Tg -41.1 - -39.4 °CASTM D7028
 -40.0 °C10°C/min; Dry; ISO 11357-1/-2
Decomposition Temperature 375 °C1% wt. loss, TGA, in air
 410 °C1% wt. loss, TGA, in nitrogen
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
Yellow Card Available; Dry; IEC 60695-11-10
 V-0
@Thickness 0.800 mm
Yellow Card Available; Dry; IEC 60695-11-10
 5VB
@Thickness 1.50 mm
IEC 60695-11-20
Oxygen Index 42 %ASTM D2863
 42 %Dry; ISO 4589-1/-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.41sodium D line; ASTM D542
 
Descriptive Properties
Form as DeliveredPowder
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema KYNAR FLEX® 2850 PC Polyvinylidene Fluoride Spray Coating Powder
Arkema Kynar Flex® 2751-00 Polyvinylidene Fluoride Powder
Arkema Kynar Flex® 2801-00 Polyvinylidene Fluoride Powder
Arkema Kynar Flex® PPA 2200 PVDF
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding

PARKG937 / 144562

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.