MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total MDPE 3802 B Medium Density Polyethylene, Cable
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: MDPE 3802 B is a black medium density polyethylene particularly suited for cable sheathing applications and designed to meet the requirements for telecommunication and power cables (medium and high voltage).

MDPE 3802 B key characteristics are

  • a superior resistance to crack formation and growth,
  • an optimal balance of flexibility and mechanical strength allowing easy coiling, handling and installation together with high surface hardness and excellent abrasion resistance,
  • an optimized formulation of additives and finely dispersed carbon black providing outstanding long-term stability in service,
  • Low dielectric constant,
  • Easy processing.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.948 g/ccISO 1183
Environmental Stress Crack Resistance >= 1000 hourF50; ASTM D1693B
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133/D
 0.90 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133/T
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60DIN 53505
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 240 °C
 
Descriptive Properties
Thermal Stability 200°C> 20 minEN 728

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Baystar™ HL 323 MDPE Medium Density Polyethylene, Film Resin
Total PPR 8650 Polypropylene, Random Copolymer
Total MDPE 3802 Medium Density Polyethylene, Cable
Total MDPE 3802 Blue Medium Density Polyethylene, Stripes
Total HP 401 MDPE, pipe, cable, sheet

PTOTAL763 / 130488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.