MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Diamond Softflex® SF 0450
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Thermoplastic Elastomer Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
Melt Flow 42 g/10 min
@Load 1.00 kg,
Temperature 235 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40 - 50ASTM D792
Tensile Strength, Yield 4.30 MPachs 2.0 in/min; ASTM D638
Elongation at Break 600 %chs 2.0 in/min; ASTM D638
Tear Strength 150 pliASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Barlog Plastics KEBAFLEX E 60.1 TPE-V, Shore A60
Avient Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE)
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
A. Schulman DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE)

PDIAM492 / 126583

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.