System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Arkema Evatane® 1006 VL 2E Ethylene Vinyl Acetate
Categories:
Polymer
;
Film
;
Thermoplastic
;
Ethylene Vinyl Acetate
;
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Material Notes:
EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 200 at 210 µm for greenhouse coverage.
ISO data provided by the manufacturer, Arkema.
Key Words:
EVAC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.925
g/cc
0.0334
lb/in³
Melt Flow
0.66
g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.66
g/10 min
@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
9.00
MPa
1310
psi
50 mm/min
Elongation at Break
>= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus
0.140
GPa
20.3
ksi
1 mm/min
Thermal Properties
Metric
English
Comments
Melting Point
104
°C
219
°F
10°C/min
Vicat Softening Point
87.0
°C
189
°F
50°C/hr; 50N
Optical Properties
Metric
English
Comments
Transmission, Visible
80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Arkema Evatane® 1020 VG 5 Ethylene Vinyl Acetate
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate
Arkema Evatane® 1020 VG 2 Ethylene Vinyl Acetate
PARKG056 / 25532
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.