MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Evatane® 1006 VL 2E Ethylene Vinyl Acetate
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 200 at 210 µm for greenhouse coverage.

ISO data provided by the manufacturer, Arkema.

Key Words: EVAC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/cc
Melt Flow 0.66 g/10 min
@Load 2.16 kg,
Temperature 190 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 9.00 MPa50 mm/min
Elongation at Break >= 50 %Nominal Strain; 50 mm/min
Tensile Modulus 0.140 GPa1 mm/min
 
Thermal PropertiesOriginal ValueComments
Melting Point 104 °C10°C/min
Vicat Softening Point 87.0 °C50°C/hr; 50N
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 80 %Mfr. reports 'Transparent' but doesn't quantify.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Evatane® 1020 VG 5 Ethylene Vinyl Acetate
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate
Arkema Evatane® 1020 VG 2 Ethylene Vinyl Acetate

PARKG056 / 25532

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.