MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Eastar DN004HF Copolyester  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Applications:
  • Displays
  • Personal care and Cosmetics

Product Description: Eastar Copolyester DN004HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to process and can fill intricate tools. Its most outstanding features are clarity, toughness and chemical resistance. DN004HF contains a mold release. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D785
Tensile Strength at Break 38.0 MPaASTM D638
Tensile Strength, Yield 47.0 MPaASTM D638
Elongation at Break 260 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Flexural Strength 65.0 MPaASTM D790
Flexural Modulus 1900 MPaASTM D790
Izod Impact, Notched 69.0 J/m
@Temperature -40.0 °C
ASTM D256
 NB
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Puncture Energy 46.0 J
@Temperature -40.0 °C
At Max load; ASTM D3763
 47.0 J
@Temperature 23.0 °C
At Max load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °CASTM D648
Vicat Softening Point 84.0 °C
@Load 1.00 kg
ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %ASTM D1003
Transmission, Visible 90 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
Mold Temperature 15.0 - 30.0 °C
Drying Temperature 71.0 °C
Dry Time 6 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Eastar DN001HF Copolyester
Eastman AP005 Copolyester
Eastman Eastar DN114 Copolyester, Natural
Eastman Eastar DN004 PCTG Copolyester
Eastman Eastar CN005 Copolyester, High Flow Grade

PE8807 / 129652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.