MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® B3WG6 HP BK 23210 30% Glass Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade with enhances flowability used e.g. for automobile manifold.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.36 g/ccISO 1183
Linear Mold Shrinkage 0.0030 cm/cm
Melt Flow 68 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDIN 58765
Decomposition Temperature >= 300 °C
Ignition Temperature >= 400 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 260 °CFeed Zone
Zone 2 270 °CCompression
Zone 3 280 °CMetering-zone
Zone 4 280 °CNozzle
Melt Temperature 270 - 290 °CInjection Molding/Extrusion
 280 °COptimal
Mold Temperature 80.0 °COptimal
 80.0 - 90.0 °CInjection Molding
Drying Temperature 80.0 °C
Dry Time 4 hour
 
Descriptive Properties
ColorBK 23210
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Conditioned)
Custom Resins Nylene® 434 Un-reinforced Nylon 6
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Dry)

PBASG0401 / 132034

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.