MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, a viscosity of 300 cps., and a weight of 7.8 lbs/gallon. AboCast 7802-1/AboCure 50-3 has versatility, many variable-ratio possibilities, and a tenacious adhesion to metals, ceramics, glass, wood, and most rigid materials which permits permanent structural and dielectric bonds. Absence of volatiles and minimum shrinkage, typical of solventless epoxy systems, allow castings and masses of virtually any desired thickness. Suggested Uses: Multi-purpose casting, coating, and bonding for applications requiring high dielectric resistance, structural strength, and radiation resistance as well as resistance to weather, water, alkalis, diluted acids, fuels, and most common solvents; it was originally developed for FERMILAB.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 lb/galAboCure 50-3
 9.10 lb/galAboCast 7802-1
Water Absorption 0.20 - 0.40 %
Viscosity 400 - 600 cPblended
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 10
@Time 86400 sec
1/8 in thickness
 30
@Time 86400 sec
 45
@Time 259000 sec
1/8 in thickness
 65
@Time 259000 sec
 65
@Treatment Temp. 100 °C,
Time 10800 sec
1/8 in thickness
 70
@Treatment Temp. 100 °C,
Time 10800 sec
Tensile Strength at Break 2000 - 3000 psi
Elongation at Break >= 20 %
Flexural Strength 2000 - 3000 psi
Compressive Strength 2000 - 3000 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 300 - 400 V/mil
 
Processing PropertiesOriginal ValueComments
Pot Life 240 min100 g
 
Descriptive Properties
Parts by Weight (pbw)100AboCast 7802-1
 80AboCure 50-13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cosmic Plastics CP7314 Epoxy Molding Compound
CHT Group EP QS EPI Engineered Polymers Quick Set Epoxy
Bostik Simple-Fix™ Hardwood Flooring Epoxy Repair Kit
BCC Products BC 5003 Epoxy Laminating System
Bakelite® EP 8413 Epoxy Molding Compound

PABC826 / 107810

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.