MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Riteflex® 655 Thermoplastic Polyester Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes:

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Water Absorption 0.40 %ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm ASTM D955
Melt Flow 7.0 - 11 g/10 min
@Temperature 220 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ASTM D2240
Tensile Strength, Ultimate 25.0 MPaASTM D638
Tensile Strength, Yield 8.90 MPa5% Yield; ASTM D638
Elongation at Break 430 %ASTM D638
Tensile Modulus 0.240 GPaASTM D638
Flexural Modulus 0.210 GPaASTM D790
Izod Impact, Notched NBASTM D256
 1.40 J/cm
@Temperature -40.0 °C
ASTM D 256
Tear Strength 150 kN/mASTM D1004
 160 kN/mASTM D624
Taber Abrasion, mg/1000 Cycles 85H-18 Wheel; 1000 g weight; ASTM D1044
 
Thermal PropertiesOriginal ValueComments
CTE, linear 198 µm/m-°C
@Temperature 20.0 °C
ASTM E831
Melting Point 200 °CASTM D1238
Maximum Service Temperature, Air 121 °C
Vicat Softening Point 181 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 221 - 238 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Riteflex® 640 Thermoplastic Polyester Elastomer (TPE)
Celanese Riteflex® 647 Thermoplastic Polyester Elastomer (TPE)
Celanese Riteflex® LX640 Satin Chrome TPZ, Unfilled
Celanese Riteflex® 635 Thermoplastic Polyester Elastomer (TPE)
Celanese Riteflex® XFR 440 TPC, Unfilled

PHCV05 / 45845

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.