MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F655 Bismaleimide Resin
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: HexPly® F655 is a bismaleimide resin that cures via an addition reaction in a toughened two-phase thermoset matrix with no condensation by-products. HexPly® F655 is a controlled flow polyimide resin system designed for alternative processing capabilities such as co-curing over honeycomb core, compression molding, as well as standard autoclave processing.

Information provided by HexCel

Key Words: BMI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/cc
Moisture Absorption at Equilibrium 4.1 %4.1 %
 
Mechanical PropertiesMetricEnglishComments
Fracture Toughness 1.37 MPa-m½1.25 ksi-in½
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  2.98
@Frequency 1.60e+10 Hz,
Temperature 24.0 °C
2.98
@Frequency 1.60e+10 Hz,
Temperature 75.2 °F
F655 Resin Casting; +/- 2%; ASTM D2520
 3.04
@Frequency 9.00e+9 Hz,
Temperature 24.0 °C
3.04
@Frequency 9.00e+9 Hz,
Temperature 75.2 °F
F655 Resin Casting; +/- 2%; ASTM D2520
 3.04
@Frequency 1.60e+10 Hz,
Temperature 149 °C
3.04
@Frequency 1.60e+10 Hz,
Temperature 300 °F
F655 Resin Casting; +/- 2%; ASTM D2520
 3.08
@Frequency 3.00e+9 Hz,
Temperature 24.0 °C
3.08
@Frequency 3.00e+9 Hz,
Temperature 75.2 °F
F655 Resin Casting; +/- 2%; ASTM D2520
 3.09
@Frequency 9.00e+9 Hz,
Temperature 149 °C
3.09
@Frequency 9.00e+9 Hz,
Temperature 300 °F
F655 Resin Casting; +/- 2%; ASTM D2520
 3.11
@Frequency 1.60e+10 Hz,
Temperature 232 °C
3.11
@Frequency 1.60e+10 Hz,
Temperature 450 °F
F655 Resin Casting; +/- 2%; ASTM D2520
 3.14
@Frequency 3.00e+9 Hz,
Temperature 149 °C
3.14
@Frequency 3.00e+9 Hz,
Temperature 300 °F
F655 Resin Casting; +/- 2%; ASTM D2520
 3.15
@Frequency 9.00e+9 Hz,
Temperature 232 °C
3.15
@Frequency 9.00e+9 Hz,
Temperature 450 °F
F655 Resin Casting; +/- 2%; ASTM D2520
 3.19
@Frequency 3.00e+9 Hz,
Temperature 232 °C
3.19
@Frequency 3.00e+9 Hz,
Temperature 450 °F
F655 Resin Casting; +/- 2%; ASTM D2520
 3.44
@Frequency 4.90e+10 Hz,
Temperature 24.0 °C
3.44
@Frequency 4.90e+10 Hz,
Temperature 75.2 °F
Astro Quartz II/F655 Dry; +/- 2%
 3.6
@Frequency 4.90e+10 Hz,
Temperature 24.0 °C
3.6
@Frequency 4.90e+10 Hz,
Temperature 75.2 °F
Astro Quartz II/F655 Wet; +/- 2%
 4.44
@Frequency 4.90e+10 Hz,
Temperature 24.0 °C
4.44
@Frequency 4.90e+10 Hz,
Temperature 75.2 °F
E-Glass/F655 Dry; +/- 2%
 4.65
@Frequency 4.90e+10 Hz,
Temperature 24.0 °C
4.65
@Frequency 4.90e+10 Hz,
Temperature 75.2 °F
E-Glass/F655 Wet; +/- 2%
Dielectric Loss Index  0.0030
@Frequency 4.90e+10 Hz,
Temperature 24.0 °C
0.0030
@Frequency 4.90e+10 Hz,
Temperature 75.2 °F
Astro Quartz II/F655 Dry; +/- 0.5
 0.0040
@Frequency 3.00e+9 Hz,
Temperature 24.0 °C
0.0040
@Frequency 3.00e+9 Hz,
Temperature 75.2 °F
F655 Resin Casting; +/- 0.5; ASTM D2520
 0.0050
@Frequency 3.00e+9 Hz,
Temperature 149 °C
0.0050
@Frequency 3.00e+9 Hz,
Temperature 300 °F
F655 Resin Casting; +/- 0.5; ASTM D2520
 0.0050
@Frequency 9.00e+9 Hz,
Temperature 24.0 °C
0.0050
@Frequency 9.00e+9 Hz,
Temperature 75.2 °F
F655 Resin Casting; +/- 0.5; ASTM D2520
 0.0060
@Frequency 3.00e+9 Hz,
Temperature 232 °C
0.0060
@Frequency 3.00e+9 Hz,
Temperature 450 °F
F655 Resin Casting; +/- 0.5; ASTM D2520
 0.0060
@Frequency 9.00e+9 Hz,
Temperature 149 °C
0.0060
@Frequency 9.00e+9 Hz,
Temperature 300 °F
F655 Resin Casting; +/- 0.5; ASTM D2520
 0.0060
@Frequency 1.60e+10 Hz,
Temperature 24.0 °C
0.0060
@Frequency 1.60e+10 Hz,
Temperature 75.2 °F
F655 Resin Casting; +/- 0.5; ASTM D2520
 0.0065
@Frequency 4.90e+10 Hz,
Temperature 24.0 °C
0.0065
@Frequency 4.90e+10 Hz,
Temperature 75.2 °F
E-Glass/F655 Dry; +/- 0.5
 0.0070
@Frequency 9.00e+9 Hz,
Temperature 232 °C
0.0070
@Frequency 9.00e+9 Hz,
Temperature 450 °F
F655 Resin Casting; +/- 0.5; ASTM D2520
 0.0070
@Frequency 1.60e+10 Hz,
Temperature 149 °C
0.0070
@Frequency 1.60e+10 Hz,
Temperature 300 °F
F655 Resin Casting; +/- 0.5; ASTM D2520
 0.0080
@Frequency 1.60e+10 Hz,
Temperature 232 °C
0.0080
@Frequency 1.60e+10 Hz,
Temperature 450 °F
F655 Resin Casting; +/- 0.5; ASTM D2520
 0.012
@Frequency 4.90e+10 Hz,
Temperature 24.0 °C
0.012
@Frequency 4.90e+10 Hz,
Temperature 75.2 °F
Astro Quartz II/F655 Wet; +/- 0.5
 0.0145
@Frequency 4.90e+10 Hz,
Temperature 24.0 °C
0.0145
@Frequency 4.90e+10 Hz,
Temperature 75.2 °F
E-Glass/F655 Wet; +/- 0.5
 
Thermal PropertiesMetricEnglishComments
CTE, linear  47.8 µm/m-°C
@Temperature 24.0 - 250 °C
26.6 µin/in-°F
@Temperature 75.2 - 482 °F
 63.2 µm/m-°C
@Temperature 175 - 250 °C
35.1 µin/in-°F
@Temperature 347 - 482 °F
Glass Transition Temp, Tg >= 204 °C>= 399 °FWet
 288 °C550 °FDry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
Hexcel® HexPly® F650 Bismaleimide Resin
Hexcel® HexPly® F652 Bismaleimide Resin
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber
Hexcel® HexPly® M65 Bismaleimide Resin

PHEXC011 / 98481

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.