MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Diamond TR 5000
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: Description: Transparent ABS

Information provided by Diamond Polymers, Inc.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 2.1 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Tensile Strength, Yield 7085 psichs 2 in/min; ASTM D638
Flexural Modulus 334000 psiProcedure B, Test Method I(chs 0.05 in/min); ASTM D790
Izod Impact, Notched 2.00 ft-lb/inTest Method A (0.125 in bar); ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 163 °F0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 4.2 %
@Thickness 3.00 mm
ASTM D1003
Transmission, Visible 88 %
@Thickness 3.00 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 374 - 482 °F
Mold Temperature 104 - 140 °FHigher mold temperature provides a product with excellent surface finishing and less residual stress.
Drying Temperature 176 - 185 °F
Dry Time 2 - 4 hour
Injection Pressure 700 - 1100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PSC 500 Polystyrene
A. Schulman Diamond ABS TR-5000 Transparent
Chevron Phillips EA3025 Crystal Polystyrene
Ineos ABS Centrex® 401 AES Extrusion
INEOS Styrolution Polystyrol 165 H GR 2 PS

PDIAM230 / 30068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.