MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos A4040 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Ineos HDPE A4040 is a high density polyethylene copolymer resin used mainly for the extrusion of crosslinked pipes according to the PEX B silane process.

Key Words: Crosslinked pipes
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.947 g/ccASTM D4883
ESCR 100% Igepal® 10 hourCondition B, F50; ASTM D1693
Oxidative Induction Time (OIT) >= 2.5 min
@Temperature 210 °C
ASTM D3895
Melt Flow 4.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ASTM D2240
Tensile Strength at Break 30.0 MPa2 in/min.; ASTM D638
Tensile Strength, Yield 24.5 MPa2 in/min.; ASTM D638
Elongation at Break >= 1270 %2 in/min.; ASTM D638
Elongation at Yield 11 %2 in/min.; ASTM D638
Flexural Modulus 0.860 GPa2% Secant; ASTM D790A
Izod Impact, Notched 1.10 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CASTM D648
Vicat Softening Point 124 °CASTM D1525
Brittleness Temperature <= -75.0 °CASTM D746
 
Descriptive Properties
processPipe Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil HD 8660.29 Rotational Molding Resin
ExxonMobil HD 5402 High Density Polyethylene Copolymer Resin
Ineos K44-15-186 Polyethylene Copolymer
Ineos K44-15-122 HDPE
Ineos K44-08-122 HDPE

PSOLKM013 / 68244

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.