MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Vanceva® Polyvinyl Butyral Interlayer
Categories: Polymer; Film

Material Notes: Vanceva® interlayers , including Vanceva Colours, Vanceva Earth Tones and Vanceva Illusion White, are Saflex R formulation products. Vanceva Colors and Vanceva Earth Tones have premium colorants uniformly distributed throughout the sheeting. Vanceva Illusion White has a white gradient band of 30 cm with a gentle fade to clear in the width of a single roll. All Vanceva products have demonstrably met or exceeded many regulations for laminated safety glazing (including those listed above) when propertly selected, laminated, and installed. Vanceva interalyers are specifically formulated to proved exceptional durability when exposed to natural weathering, especially when laminate edges are left unprotected from the elements. Vanceva interlayers have been shown to be compatible and durable when laminated in intimate contact with most infrared reflective, metal coated glasses.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5252cut/stacked to 12.5 mm; ASTM D2240
Tensile Strength at Break 27.0 MPa3920 psiJIS 56771
Elongation at Break 205 %205 %JIS K6771
Modulus of Elasticity 0.00156 GPa
@Temperature 60.0 °C
0.226 ksi
@Temperature 140 °F
1 Hz
Poissons Ratio 0.500.50ASTM D638
Tear Strength 0.00112 kN/m0.00639 pli
 
Thermal PropertiesMetricEnglishComments
CTE, linear 155 µm/m-°C
@Temperature 30.0 - 100 °C
86.1 µin/in-°F
@Temperature 86.0 - 212 °F
ASTM E831
Specific Heat Capacity 1.98 J/g-°C
@Temperature 50.0 °C
0.473 BTU/lb-°F
@Temperature 122 °F
ASTM E1269
Thermal Conductivity 0.200 W/m-K
@Temperature 65.0 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 149 °F
ASTM F433
Glass Transition Temp, Tg 29.0 - 31.0 °C84.2 - 87.8 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4781.478ASTM D542
Haze <= 1.0 %<= 1.0 %Clear 3 mm Glass; ASTM D1003
Yellow Index <= 1.0 %<= 1.0 %Clear 3 mm Glass; ASTM E313
Transmission, Visible 89 %89 %clear 3 mm Glass; NFRC 300
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.00 - 0.050 %0.00 - 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Butvar® B-72 Polyvinyl Butyral Resin
Eastman Butvar® B-98 Polyvinyl Butyral Resin
Cobalt, Co
Beryllium, Be
Overview of materials for Very Low Density Polyethylene (VLDPE)

PEATM5541 / 222735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.