MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing
Categories: Polymer; Thermoplastic

Material Notes: Tygon S3™ E-3603 from Saint-Gobain Performance Plastics is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable, flexible tubing products. The bio-based Tygon S3™ line combines the high performance standards customers demand with an eco-friendly tubing design. Crystal-clear and flexible, Tygon S3™ E-3603 non-DEHP tubing delivers the same superior performance you have come to expect, but now in a formulation that contains a non-DEHP plasticizer.

Tygon S3™ E-3603 tubing handles most inorganic chemicals found in the laboratory. It is non-oxidizing and non-contaminating, and less permeable than rubber tubing. The glassy-smooth inner bore helps prevent buildup to facilitate cleaning. Coils are marked at 1-foot (30.4 cm) intervals for easy measuring.

Applications include analytical instruments, general laboratory, Peristaltic and vacuum pumps, biopharmaceutical, incubators, desiccators, gas lines, and food and beverage.

Features and Benefits

  • New bio-based formulation delivers the same excellent performance
  • Outstanding chemical resistance
  • Lot-to-lot consistency for reproducible results
  • Non-oxidizing and non-contaminating
  • Contains no BPA or phthalates
  • Standard sizes available to hold full vacuum at room temperature
  • Smooth, polished inner wall
  • Slips easily over fittings and grips securely for simple lab set-ups

Regulatory Information: Tygon S3™ complies with FDA, NSF, 3-A, Japan Food Sanitation Law # 370/1959, REACH, 1935/2004/EC and 10/2011/EU for many foods and beverages. Tygon S3™ tubing products do not contain chemicals listed in California's Prop 65.

Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM placques or molded ASTM durometer buttons.

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Water Absorption 0.21 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 56
@Time 15.0 sec
ASTM D2240
Tensile Strength 1750 psiASTM D412
Tensile Stress at Strain 582 psi
@Strain 100 %
Elongation at Break 425 %ASTM D412
Tear Strength 173 pliASTM D1004
Compression Set 64 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395 Method B
Tensile Set 95 %at 75% Elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °F
Brittleness Temperature -51.0 °FASTM D746
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Clear, but value not quantified
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
FDA Yes
NSF Yes
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation
Saint-Gobain Tygon® S3™ B-44-4X Phthalate-free Food, Milk, and Dairy tubing
Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture
Saint-Gobain Tygon® S3™ B-44-3 Bio-based Beverage Tubing Formulation
Saint-Gobain Norton® Tygon® R-3603 Laboratory and Vacuum Tubing Formulation

PSTGQ908 / 160404

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.