MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Niagara LaSalle Fatigue-Proof® Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel

Material Notes: Fatigue-Proof® has the high strength properties usually associated only with heat treated steels. It also has excellent machining characteristics, resistance to fatigue and corresponds to AISI Grade 1144. From this special quality hot roll grade Fatigue-Proof® is made by various combinations of mechanical working and thermal treatment wear, and it minimizes distortion. Fatigue-Proof® is produced from a high manganese, resulfurized, silicon killed steel.

Information provided by Niagra LaSalle Corporation

Key Words: AISI 1144
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell >= 285>= 285
Hardness, Rockwell C >= 30>= 30
Tensile Strength >= 965 MPa>= 140000 psi
Tensile Strength, Yield >= 862 MPa>= 125000 psi
Elongation at Break >= 5.0 %>= 5.0 %
Reduction of Area >= 15 %>= 15 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.40 - 0.48 %0.40 - 0.48 %
Iron, Fe 96.79 - 97.86 %96.79 - 97.86 %as balance
Manganese, Mn 1.35 - 1.65 %1.35 - 1.65 %
Phosphorus, P <= 0.40 %<= 0.40 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S 0.24 - 0.33 %0.24 - 0.33 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Niagara LaSalle StressProof® Cold Finished Steel Bar
AISI 1144 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1144 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Niagara LaSalle 1144 Cold Finished Steel Bar
440C Martensitic Stainless Steel (UNS S44004)

NNIAL004 / 160294

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.