MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ SC-102 Unfilled Silicone Encapsulant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Lord SC-102 is a "water-white" clear, two component, silicone encapsulating system. It has a very low viscosity and, when cured, a low Shore A hardness. Lord SC-102 is optically transparent with no yellowish tint. It offers excellent protection for delicate components against vibration, mechanical and thermal shock, and moisture while producing a soft, tack-free surface. This material was formulated for use in electrical and electronic potting applications where ease of repair is a necessity. Lord SC-102 can be easily cut open with a knife.

Lord SC-102 is addition curing. It will not depolymerize when heated in confined spaces as do many condensation curing silicones. As with all silicones, SC-102 generates no exotherm as it cures. It also exhibits low shrinkage and stress on components as it cures. Lord SC-102's cure may be accelerated with elevated temperature.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccSTM 2
Viscosity 380 cPSTM 1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 26ASTM D2240
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.50e+15 ohm-cm
@Temperature 25.0 °C
ASTM D257
Dielectric Constant 2.96
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150
Dielectric Strength 440 V/milASTM D149
Dissipation Factor 0.0028
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 480 µm/m-°CCalculated from Volume CTE; ASTM D864
Thermal Conductivity 0.146 W/m-KASTM D2214
Maximum Service Temperature, Air 200 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 10.0 min
@Temperature 100 °C
 15.0 - 20.0 min
@Temperature 60.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 30 - 40 min
@Temperature 25.0 °C
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
AppearanceClear
Mix Ratio1:1by weight, by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® 5071 Silicone Encapsulant
Lord Adhesives Circalok™ 6715 Silicone Encapsulant
Lord Adhesives Thermoset™ SC-300M Silicone Gel Encapsulant
Lord Adhesives Thermoset™ SC-309 Thermally Conductive Silicone Encapsulating System
Dow JCR 6110 A/B

PLORD063 / 86071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.