MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 8617 Steel, heat treated, machined, pseudocarburized, 150°C (300°F) temper
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: Normalized 925°C (1700°F) in 32 mm rounds, machined to 25 or 13.7 mm rounds, pseudocarburized at 925°C (1700°F) for 8 hours, oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds. Post oil quenched hardness 25 mm: 302 HB at 7/8 radius, 265 HB at half-radius, 258 HB at center; 50 mm: 235 HB at 7/8 radius, 215 HB at half-radius, 207 HB at center

Key Words: DIN 1.6523, AFNOR 20 NCD 2 (Fr), AFNOR 22 NCD 2 (Fr), UNI NiCrMo 2, JIS SNCM 21 H, JIS SNCM 21, B.S. 805 H 20, B.S. 805 M 20, UNS G86170, ASTM A322, ASTM A331, ASTM A505, AMS 6272, SAE J404, SAE J770
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 255
Hardness, Knoop 279Converted from Brinell
Hardness, Rockwell B 98Converted from Brinell
Hardness, Rockwell C 25Converted from Brinell
Hardness, Vickers 269Converted from Brinell
Tensile Strength, Ultimate 883 MPa
Tensile Strength, Yield 650 MPa
Elongation at Break 19 %in 50 mm
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steels
Poissons Ratio 0.29Calculated
Machinability 70 %hot rolled and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPaTypical for steel.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000234 ohm-cmTypical steel
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.475 J/g-°CTypical steel
Thermal Conductivity 46.6 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.15 - 0.20 %
Chromium, Cr 0.40 - 0.60 %
Iron, Fe 96.975 - 98.05 %As remainder
Manganese, Mn 0.70 - 0.90 %
Molybdenum, Mo 0.15 - 0.25 %
Nickel, Ni 0.40 - 0.70 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.30 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 8617H Steel, heat treated, machined, pseudocarburized, 150°C (300°F) temper
AISI 8617 Steel, heat treated, machined, pseudocarburized, reheated to 855°C (1570°F), 150°C (300°F) temper
AISI 8617H Steel, heat treated, machined, pseudocarburized, reheated to 800°C (1470°F), 150°C (300°F) temper
AISI 8617H Steel, heat treated, machined, pseudocarburized, reheated to 855°C (1570°F), 150°C (300°F) temper
AISI 8617 Steel, double quenched, 150°C (300°F) temper

M861BA / 8273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.