MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics V-19 Block Insulation
Categories: Ceramic

Material Notes: V-19 Block is manufactured from vermiculite granules and high-temperature bonding materials. This versatile product is available in thicknesses up to 4".

V-19 Block is an economical, energy saving insulation with minimal shrinkage at its top temperature limit, and good compressive strength. These features make V-19 a good design choice for back-up insulation applications.

V-19 compositional characteristics permits effective adhesion of cement finishes. Therm-O-Stix is an ideal adhesive product with superior qualities when used with V-19.

V-19 Block must be pre-drilled for placement since it is not impalable over anchors due to its high green strength. However this property makes it easy to cast or gun against with refractory castables.

Features:

  • Economical structural insulation
  • 1900°F (1038°C) temperature rating
  • Low thermal conductivity
  • No organic binders or fillers
  • Manufactured to close dimensional tolerances, max. ± 1/16”
  • Volumetric stable to use limit
  • Alternative to mineral wool board
  • Applications:

  • Back-up insulation in all industries
  • Suitable for use with castables, firebrick, refractory plastic and ceramic fiber

    Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.3845 g/ccat ambient temperature; ASTM C303
     0.3925 g/cc
    @Temperature 1040 °C
    ASTM C303
    Porosity 93 %ASTM C493
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Rupture 0.110 ksiat ambient temperature; ASTM C203
     0.0750 ksi
    @Temperature 1040 °C
    ASTM C203
    Compressive Strength 1.137 MPaat ambient temperature; ASTM C165
     0.5515 MPa
    @Temperature 1040 °C
    ASTM C165
     
    Thermal PropertiesOriginal ValueComments
    Specific Heat Capacity 0.840 J/g-°C
    Thermal Conductivity 0.110 W/m-K
    @Temperature 260 °C
     0.130 W/m-K
    @Temperature 538 °C
     0.150 W/m-K
    @Temperature 816 °C
    Maximum Service Temperature, Air 1900 °FContinuous
     2300 °FRating
    Shrinkage 2.3 %
    @Temperature 1040 °C
    Linear; ASTM C356
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 10.1 %
    Alkalis 2.9 %
    CaO 17 %
    Fe2O3 7.6 %
    MgO 14.5 %
    SiO2 44 %
    TiO2 1.3 %
     
    Descriptive Properties
    Sulfur Trioxide Content, %0.5

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Centro Plastica CiPiTENE® Recycled High Density Polyethylene Granules
    LATI LATISHIELD 87/28-06A Polycarbonate E.M.I. Shielding Plastic
    Pyrotek U-1 Compressible Board
    Pyrotek Firefly 800 Roller & Furnace Cladding Material
    Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic

    CTHERM024 / 2344

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.