MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Black
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thus will support a wide and flexible range of products.

Flame retardant compounds will extend the application areas where resistance to ignition and burning are important features, while their performance characteristics in processing and finished component operation are of the same standard a the Dryflex® general-purpose grades.

The flame retardant compounds show an excellent resistance to a variety of polar fluids, such as water, aqueous systems and alcohols. However, in non-polar fluids, such as oil, resistance diminishes with increasing aromatic content. Weathering, including UV stability and ozone resistance is excellent.

Processing: The flame retardant grades of Dryflex® can easily be processed using conventional thermoplastic equipment for injection molding as well as other fabricating methods. The thermoplastic characteristics result in faster processing times and complete scrap recycling. The flame retardant compounds do not require pre-drying prior to processing.

Information from Vita Thermoplastic Polymers (VTP).

Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/ccISO 2781
Melt Flow 2.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ISO 868
Tensile Strength at Break 5.80 MPaISO 37
Elongation at Break 300 %ISO 37
100% Modulus 0.00440 GPa
@Strain 100 %
ISO 37
Tear Strength 35.0 kN/mMethod C; ISO 34
Compression Set 30 %
@Temperature 23.0 °C,
Time 86400 sec
Method B; ISO 815
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE)
Barlog Plastics KEBAFLEX S 95 A.01 TPE-S, Shore A95, translucent
Teknor Apex Laripur® LPR 9060EF Thermoplastic Polyurethane
Samyang Triel® 5302FR Thermoplastics Polyetherester Elastomer, Non-Halogen Flame Retardancy
Huntsman IROGRAN® A 92 E 4670 TPU-Polyester

PVTC010 / 72079

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.