MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Riteflex® XFR 655 TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex XFR 655 is a thermoplastic polyester elastomer featuring a halogen-free flame redardant system and is UL certified to be V-0 at 1.5 mm in all colors. It has shore D hardness of 55 and an excellent balance of mechanical properties, flame retardant efficiency and processability.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccISO 1183
Melt Flow 8.7 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 20 g/10 min
@Load 2.16 kg,
Temperature 250 °C
[cm3/10min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5515 sec; ISO 868
Tensile Strength at Break 16.0 MPa50mm/min; ISO 527-2/1A
Tensile Stress at Strain 14.0 MPa
@Strain 50 %
ISO 527-2/1A
Elongation at Break >= 50 %
 250 %50mm/min; ISO 527-2/1A
Tensile Modulus 360 MPa50mm/min; ISO 527-2/1A
Charpy Impact, Notched 13.0 kJ/m²ISO 179/1eA
Tear Strength 55.0 kN/mISO 34-1
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 15.0 kV/mmIEC 60243-1
Comparative Tracking Index >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 °C10°C/min; ISO 11357-1,-2,-3
Flammability, UL94 V-0
@Thickness 1.50 mm
Oxygen Index 37.2 %ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Riteflex® 655 Thermoplastic Polyester Elastomer (TPE)
Celanese Riteflex® 677 TPC, Unfilled
Celanese Riteflex® UV655M TPC, Unfilled
Celanese Riteflex® XFR 440 TPC, Unfilled
Celanese Riteflex® 635 Thermoplastic Polyester Elastomer (TPE)

PHCQ461 / 178916

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.