MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unipetrol Grade D Diesel Oil
Categories: Fluid; Solvent

Material Notes: Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their application characteristics such as depressants, detergents, lubrication additives and corrosion inhibitors. Diesel oils are used as fuel for diesel engines or fuel for some types of gas turbines as well.

Information provided by Unipetrol RPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.820 - 0.845 g/cc
@Temperature 15.0 °C
Viscosity Measure 2.0 - 4.5 cSt
Ash <= 0.010 %
Evaporation Loss <= 65 %
@Temperature 250 °C
 >= 85 %
@Temperature 350 °C
 >= 95 %
@Temperature 360 °C
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 55.0 °Cnad
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.020 %
 
Component Elements PropertiesOriginal ValueComments
Sulfur, S 0.0050 %
 
Descriptive Properties
Cetane index, min46
Cetane Number, min51
Oxidative Stability, g/cc, max25
Total Impurity Content %, max0.0024

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco 13 SG Diesel Engine Oil
ChevronTexaco 17 MG 2000 Diesel Engine Oil
ChevronTexaco 17 SG 2000 Diesel Engine Oil
ChevronTexaco DIESELMOTIVE® Direct Injector Cleaner, for Heavy Duty Diesel Engines
Unipetrol Grade B Diesel Oil

PUNIP079 / 82939

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.