MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, and oil and gas industry, PVDF is also gaining recognition in automotive, building, electronics, pharmaceutical and batteries. 3M™ Dyneon™ PVDF 1008/0001 is easily processed under a variety of conventional thermoplastic conversion techniques, being particularly suitable for injection molding. Dyneon PVDF 1008/0001 is inherently pure and chemically resistant against a variety of aggressive fluids and solvents. PVDF 1008/0001 exhibits excellent dimensional stability, abrasion resistance and high strength, and maintains its mechanical properties at elevated temperature. These products are supplied in pellet form utilizing high purity packaging techniques.
  • Excellent chemical resistance to a variety of aggressive fluids and solvents
  • Good permeation resistance
  • Injection molding grade
  • Excellent strength and dimensional stability

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.78 g/ccISO 1183
Water Absorption <= 0.040 %24 hr @ 23°C; ISO 62 (method 1)
Linear Mold Shrinkage 0.030 cm/cm
Melt Index of Compound 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 24 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 42.0 MPaASTM D638
Tensile Strength, Yield 55.0 MPa50mm/min; ASTM D638
Elongation at Break 35 %ASTM D638
Elongation at Yield 7.0 %50mm/min; ASTM D638
Flexural Modulus 2.20 GPa2mm/min; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 174 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 148 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
Flammability, UL94 V-0
Oxygen Index >= 44 %ASTM D2863
 
Descriptive Properties
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill® PVDF CF10 BK 10% Carbon Filled
Celanese Riteflex® 635 Thermoplastic Polyester Elastomer (TPE)
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer

PDYNE055 / 34863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.