MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® B 50H1 Natural L PA 66/6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Description: TECHNYL® B 50H1 Natural L is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is available in natural and other colors upon request.

Key Properties: UL94 V0 at 0.4mm; High ductility at low temperature; Excellent filling qualities

Benefits: This phosphorus and halogen free flame retardant grade, UL94 V0 at 0.4mm, offers excellent filling qualities together with good stiffness.

Applications: Connectivity : junction blocks, terminal blocks, connectors.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183/A
Water Absorption 1.1 %
@Time 86400 sec
1.1 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.011 cm/cm0.011 in/inIsotropy
Linear Mold Shrinkage, Flow 0.011 cm/cm0.011 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiISO 527 Type 1A
Tensile Strength, Yield 40.0 MPa5800 psiISO 527 Type 1A
Elongation at Break 100 %100 %ISO 527 Type 1A
Elongation at Yield 5.0 %5.0 %ISO 527 Type 1A
Tensile Modulus 2.20 GPa319 ksiISO 527 Type 1A
Flexural Strength 70.0 MPa10200 psiISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²3.09 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 4.04.0IEC 60250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243
Dissipation Factor 0.0600.060IEC 60250
Comparative Tracking Index 600 V600 VSol A; IEC 60112
 600 V600 VSol B; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 242 °C468 °FISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH50
Domo TECHNYL® B 50 H1 PA66/6, DRY
Domo Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0
Domo TECHNYL® B 50H1 Natural L PA 66/6, Dry
Domo TECHNYL® B 50 H1 PA66/6, Conditioned

PSOLVAY854 / 218582

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.