MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled; Filled/Reinforced Thermoset

Material Notes: Long glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type GDI-30F.

Information provided by Vyncolit, a Sumitomo Bakelite Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.76 g/ccRelative Density; ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cmCompression Molding; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaASTM D638
Flexural Strength 110 MPaAt Rupture; ASTM D790
Flexural Modulus 20.0 GPaASTM D790
Compressive Strength 140 MPaASTM D695
Izod Impact, Notched 170 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.5
@Frequency 1e+6 Hz
Wet; ASTM D150
 4.1
@Frequency 1000 Hz
wet; ASTM D150
Dielectric Strength 13.4 kV/mm60Hz, Step-by-Step, wet; ASTM D149
Dissipation Factor 0.010
@Frequency 1000 Hz
wet; ASTM D150
 0.018
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 130 secASTM D495
Comparative Tracking Index >= 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C
@Temperature 20.0 °C
ASTM E-831
Maximum Service Temperature, Air 130 °CUL 746B
Deflection Temperature at 1.8 MPa (264 psi) 260 °CAs molded; ASTM D648
Flammability, UL94 V-0
@Thickness 3.20 mm
Oxygen Index 30 %ASTM D2863
 
Descriptive Properties
ColorBlack, Gray, Green
Flammability: Burning, sec40ASTM D229
Flammability: Ignition, sec110ASTM D229
FormCoarse Flake
Main FillerGlass Fiber
Molding MethodCompression, transfer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate
Sumitomo Bakelite North America RX® 3-2-530-P Long-Glass Reinforced Diallyl Phthalate
Sumitomo Bakelite RX® 1310 Diallyl Ortho-Phthalate Molding Compound
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled

PVYNC062 / 72270

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.