MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP38FLAO Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Thermally conductive
  • Electrically insulative
  • High flexibility
  • Very long open time
  • Cures at room or elevated temperatures
  • Excellent flowability
Product Description: Master Bond EP38FLAO is a versatile two component thermally conductive, electrically insulating epoxy. This epoxy can be used for high performance bonding, sealing, coating, potting and encapsulation. This system features a convenient and forgiving one to one mix ratio by weight or volume. It has an exceptionally long working life as well. This in and of itself is highly attractive, but add to this that it is a lower exotherm system with splendid flow, which enables it to be used in all kinds of potting and encapsulation applications, particularly those that are larger in size. Also noteworthy are its outstanding thermal conductivity, superior electrical insulation properties along with a substantial degree of flexibility. Its top notch flexibility allows it to withstand rigorous thermal cycling as well as mechanical and thermal shocks. EP38FLAO bonds well to a wide variety of substrates such as metals, glass, ceramics, composites, many rubbers and plastics, and is an excellent adhesive. It has reasonably good chemical resistance to water, oils and many fuels. It has a wide service temperature range of -100°F to 250°F. Parts A and B are off white in color. This multifaceted system is widely used in the electronic, electrical, computer, aerospace, opto-electronic and specialty OEM applications where electrical insulation and heat transfer are required and excellent flow properties are desirable. EP38FLAO is particularly special because it possesses a high level of flexibility and thermal conductivity while it retains the desirable physical characteristics inherent in epoxies.

Product Advantages:

  • Convenient mixing: easy to use, non-critical one to one mix ratio by weight or volume
  • High thermal conductivity with striking electrical insulation properties
  • Superior bond strength to a wide variety of substrates
  • Low exotherm and a long working life
  • Excellent flowability well suited for all kinds of potting and encapsulations
  • Capable of withstanding rigorous thermal cycling and shocks

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 6000 - 20000 cPPart B
 8000 - 20000 cPmixed
 20000 - 80000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75 - 85
Hardness, Shore D 30 - 40
Tensile Strength >= 4000 psi
Adhesive Bond Strength >= 850 psiTensile lap, Aluminum to Aluminum
Peel Strength >= 10.0 pli
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 4.8
@Frequency 60 Hz
Dielectric Strength 450 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 65.0 µm/m-°C
Thermal Conductivity 1.2987 - 1.4423 W/m-K
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.50 - 3.50 hour
@Temperature 93.3 °C
 72.0 - 96.0 hour
@Temperature 23.9 °C
Working Life 110 - 150 minAfter mixing, 100 g batch
Shelf Life 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Mixing Ratio1:1 by weight or volumeParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP90FR-HFL Two Component Epoxy
Master Bond EP30FL Low Viscosity, Flexibilized Two Component Epoxy
Master Bond EP21TDC-2LOND Two Component Epoxy
Master Bond EP42HT-2AO Two Component, Thermally Conductive, Heat Resistant Epoxy
Master Bond MasterSil 152 Silicone

PMASTM874 / 185467

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.