Key Features:- Exceptionally low viscosity
- Good flexibility
- Cures at room temperature
- Cryogenic serviceability
Product Description: Master Bond EP30FL is a low viscosity, two component epoxy system for high performance potting and encapsulation as well as for bonding and sealing. It is formulated to cure at room temperature or more rapidly at elevated temperatures, with a four to one mix ratio by weight. This compound is 100% reactive and does not contain any solvents or other volatiles. Most significantly, it cures remarkably more flexible than “typical” epoxies and is recommended in situations where resistance to mechanical shock and vibration as well as thermal shock and thermal cycling is needed. EP30FL can also be used as an adhesive or coating. It has very low shrinkage upon curing. It is serviceable over the exceptionally broad temperature range of 4K to +250°F, making it suitable for cryogenic applications. The system offers excellent adhesion to both similar and dissimilar materials including metals, glass, ceramics and many rubbers and plastics. It withstands a variety of chemicals including water, oil and fuels. The hardened compound is a superior electrical insulator. The color of Part A is amber and Part B is clear. EP30FL is widely used in the electronic, electro-optic, aerospace, specialty OEM and related industries.Product Advantages: - Easy application, very low viscosity; well suited for potting and encapsulating
- Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required
- Superior thermal shock resistance and thermal cycling properties
- Excellent electrical insulation properties
- Superb impact resistance and mechanical shock resistance
Information provided by Master Bond Inc. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |