MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Thermally conductive
  • Electrically insulative
  • Low thermal expansion coefficient
  • NASA approved for low outgassing applications
  • Low viscosity with excellent flowability
  • Superior dimensional stability
Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring exceptionally high thermal conductivity, excellent electrical insulation properties and NASA low outgassing approval. It will cure at room temperature or more rapidly at elevated temperatures. Other attractive properties include superb dimensional stability and superior physical strength properties. Its low viscosity and excellent flow characteristics make it an ideal thermally conductive potting epoxy. EP30AN-1 is also an excellent adhesive/ sealant forming durable, rigid bonds that resist to thermal cycling and chemicals including water, oils, etc. over the wide temperature range of -60°F to +250°F. The coefficient of thermal expansion is desirably low. The color of Part A is gray and Part B is clear. Master Bond EP30AN-1 is widely used in applications where thermal conductivity, electrical isolation and low outgassing properties are required. It is particularly well suited to high vacuum environments.

Product Advantages:

  • Easy application: adhesive spreads or pours evenly and smoothly.
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required.
  • High bond strength to a wide variety of substrates; excellent adhesive properties.
  • Exceptionally high thermal conductivity with excellent electrical insulation properties.
  • Good physical strength characteristics; especially high compressive strength.
  • Meets NASA low outgassing specifications

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 300 - 400 cP300 - 400 cPPart B
 10000 - 18000 cP10000 - 18000 cPPart A
Outgassing - Total Mass Loss 0.82 %0.82 %TML
Collected Volatile Condensable Material 0.020 %0.020 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85 - 9085 - 90
Tensile Strength 34.5 - 41.4 MPa5000 - 6000 psi
Compressive Strength 165 - 179 MPa24000 - 26000 psi
Adhesive Bond Strength 4.83 - 6.21 MPa700 - 900 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.80e+14 ohm-cm4.80e+14 ohm-cm
Dielectric Constant 4.7
@Frequency 60 Hz
4.7
@Frequency 60 Hz
Dielectric Strength >= 15.7 kV/mm
@Thickness 3.17 mm
>= 400 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 22.0 µm/m-°C11.1 - 12.2 µin/in-°F
Thermal Conductivity 3.31 - 3.6057 W/m-K23.0 - 25.024 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
 2880 - 4320 min
@Temperature 23.9 °C
48.0 - 72.0 hour
@Temperature 75.0 °F
Working Life 30.0 - 45.0 min30.0 - 45.0 minAfter mixing, 100 g batch
Shelf Life 6.00 Month
@Temperature <=23.9 °C
6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
Mixing Ratio10:1 by weightParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP37-3FLFAO Low Outgassing Thermally Conductive Epoxy System
Master Bond Supreme 10AOHT Thermally Conductive One Component Epoxy System
Master Bond EP21TDC-2 Highly Flexible Cryogenic Epoxy Compound
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Master Bond EP30FL Low Viscosity, Flexibilized Two Component Epoxy

PMASTM855 / 185448

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.