MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Amodel® FC-1150 is an FDA compliant, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good hydrolytic stability to make it particularly suited for components used in food service and consumer applications such coffee machines and ovens.

- Natural: FC-1150 NT

- Black: FC-1150 BK 946

Chemical Resistant; Chlorine Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; High Stiffness; High Strength; High Temperature Strength; Low Moisture Absorption

Uses: Appliances; Housings; Non-specific Food Applications; Plumbing Parts; Pump Parts

Processing: Injection Molding

Agency Ratings: EU 10/2011; FDA 21 CFR 176.170(c); NSF STD-51

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.67 g/ccMethod A; ISO 1183
 1.67 g/ccMethod A; ISO 1183
Linear Mold Shrinkage, Flow 0.0015 - 0.0018 cm/cm
@Thickness 2.00 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0042 cm/cm
@Thickness 2.00 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 270 MPaISO 527-2
Elongation at Break 2.0 %ISO 527-2
Tensile Modulus 19100 MPaISO 527-2
Flexural Strength 400 MPaISO 178
Flexural Modulus 18400 MPaISO 178
Charpy Impact Unnotched 88.0 kJ/m²ISO 179
Charpy Impact, Notched 12.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 300 °CFlatwise; Unannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 315 - 330 °C
Middle Barrel Temperature 320 - 340 °C
Front Barrel Temperature 325 - 345 °C
Melt Temperature 340 - 360 °C
Mold Temperature 160 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content 0.030 - 0.060 %
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorBlack; Natural
FormsPellets
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mueller Ecostream™ C36500 Uninhibited Leaded Muntz Metal
Borealis RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems
Borealis RA130E-1498 Polypropylene Random Copolymer
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic
Schmolz + Bickenbach CorroPlast® Plastic Mold Steel

PSOL8Y6083 / 193004

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.