MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Armstrong A-661 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: A truly unique, two-component, room temperature curing thixotropic epoxy adhesive system, which exhibits good bond strength at service temperatures up to 400°F. Ideal for applications where resistance to high service temperatures is required, but where a room temperature cure is desirable.

Information provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82
Tensile Strength, Ultimate 6350 psiafter optimum cure
Elongation at Break 2.5 %
Adhesive Bond Strength 5050 psiSteel-Steel; after optimum cure
 2500 psi
@Temperature -54.4 °C
Aluminum-Aluminum tensile shear
 3300 psi
@Temperature 82.2 °C
Aluminum-Aluminum tensile shear
 3900 psi
@Temperature 25.0 °C
Aluminum-Aluminum tensile shear
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 400 °F
Glass Transition Temp, Tg 115 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 72.0 °F
 300 °FOptimum cure is 10 min. @ 300°F
Pot Life <= 180 min
@Temperature 25.0 °C
100 g
 
Descriptive Properties
ColorOff White
Mix Ratio4/1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Devcon Wear Guard (High Temp) Epoxy
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Momentive Performance Materials RTV5222 White Adhesive Sealant, Low Modulus Paste
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating
Atom Adhesives AA-DUCT 2924 Epoxy Adhesive

PARM23 / 24555

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.