MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® B 238 Black 21 N PA66/6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.

Available in: Europe

Product Applications: TECHNYL B 238 is particularly recommended for applications where high thermal stress rates and good impact resistance are required, also for parts which could break during assembly or parts used at low humidity level. This grade is commonly used in: automotive industry for under bonnet fasteners. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaISO 527 Type 1A
Tensile Strength, Yield 40.0 MPaISO 527 type 1 A
Elongation at Break 250 %ISO 527 Type 1A
Elongation at Yield 12 %ISO 527 type 1 A
Tensile Modulus 900 MPaISO 527 Type 1A
Flexural Strength 27.0 MPaISO 178
Flexural Modulus 700 MPaISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²ISO 180/1eA
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 30.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Dielectric Strength 30.0 kV/mmIEC 60243
Dissipation Factor 0.070IEC 60250
Comparative Tracking Index 500 VSolution A; IEC 60112
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® B 230 PA66/6, Conditioned
Ashley Polymers Ashlene® 747 Nylon 6/66
Domo TECHNYL® A 258P1 Black 2N PA 66, Dry
Domo Technyl® A 402 H1 Nylon 66
Domo TECHNYL® B 230 Black-H PA 66/6, Conditioned

PRHOD746 / 137977

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.