MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
BCC Products BC 5105 Epoxy Laminating System
Categories: Polymer; Thermoset; Epoxy

Material Notes: BC 5105 is a clear, unfilled, low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. For use above 150ºF a post-cure may be required. BC 5105 can afford consistent use to 300ºF if required. Does not contain VCHD or MDA. Uses: constructing vacuum form tools, injection and compression molds, RTM and RIM molds, and matched dies.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Brookfield Viscosity 2000 cP
@Temperature 23.9 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
@Temperature 23.9 °C
Tensile Strength, Ultimate 29000 psi10 oz glass cloth laminate
Flexural Strength 34000 psi10 oz glass cloth laminate
Compressive Strength 58600 psi10 oz glass cloth laminate
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µin/in-°F10 oz glass cloth laminate
Deflection Temperature at 1.8 MPa (264 psi) 293 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1440 min
@Temperature 24.0 °C
Pot Life 55 min
@Temperature 24.0 °C
 
Descriptive Properties
Mix Ratio100:17 by weight, 100:20 by volume, resin/harder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites LYTEX® 4084 63% Glass Fiber Reinforced Epoxy SMC
Polybutadiene Rubber (BR)
Overview of materials for Phenolic/Glass Fiber SMC
Jushi UD1200 Glass Fiber Epoxy Composite
Dow SE SLR-4400 Solution polymerized Styrene Butadiene Rubber (S-SBR)

PBCC022 / 107249

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.