NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification and dehumidification applications such as water management and breathable fabrics. They have a high resistance to chlorine, making water treatment a target market. This data sheet is for solution, but MD9150 is also available as a cast membrane. Information provided by Kraton®. |