MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Morgan Advanced Ceramics Vacupor® NT Porextherm
Categories: Ceramic

Material Notes: Vacupor® NT is a microporous insulation material which has an extremely low thermal conductivity coefficient giving it very good insulating properties. Vacupor® NT consists of inorganic oxides. The main constituent is fumed silica, the other components are opacifiers for minimizing infrared radiation, and silicates. Vacupor® NT (core material) is not flammable and meets the requirements of IMO FTPC part 1 and DIN ISO 4102 part 1, A1. Vacupor® NT is heat sealed under vacuum in a multilayer vacuum metalized film. The very low internal pressure and the microporous panel core enable it to reach extremely low thermal conductivity values.

Application: Vacupor® NT was specially developed for applications in vacuum insulation technology. The low density and the specially developed IR opacifiers contained in these grades greatly reduce the thermal conductivity of Vacupor® NT Systems.

Typical applications: Vacupor® NT is also successfully used as insulation material in the following areas:

  • Domestic appliances (refrigerator and freezer cabinets)
  • Absorption refrigerators
  • Cryogenic freezer
  • Temperature controlled packaging
  • Transport boxes
  • Facade elements
  • Terrace insulation
  • Cold storage floor insulation
.

Information provided by Morgan Advanced Materials

Vendors:
Available Properties
  • Density, dependent on board thickness
  • Thermal Conductivity, at 1 mbar, dependent on the panel size and thickness, internal pressure can be between 0.5-5mbar. The standard internal pressure in the evacuation chamber is <0.5mbar
  • Thermal Conductivity, at ambient pressure
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air, The limits are fixed by the barrier film (sealing material) used; constant load: =<80°C; short load time with 120°C, roughly 30minutes.
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.