MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Quadrant Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistance.
  • Thermal stability in the range -76 °C up to +160 °C / -105 °F up to + 356 °F
  • Excellent chemical resistance against highly concentrated chemicals, even for a broad range of alcalines (up to pH 14)
  • Low permeability to liquids, gases and vapors.
  • High elongation at break
  • Excellent impact resistance
  • Good resistance to stress cracking, even with caustic solutions, chlorine and alkaline areas
  • Excellent weather proof and radiation proof
  • Low coefficient of thermal expansion

In January 2016 the Symalit® Fluoroplastics production assets were sold to AGRU Kunststofftechnik GmbH

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Moisture Absorption at Equilibrium, 50% RH
  • Water Absorption at Saturation
  • Hardness, Rockwell R, ISO 2039-2
  • Hardness, Shore D
  • Ball Indentation Hardness, ISO 2039-1
  • Tensile Strength, Yield, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2
  • Elongation at Yield, ISO 527-1/-2
  • Tensile Modulus, ISO 527-1/-2
  • Flexural Strength
  • Compressive Strength, ISO 604
  • Compressive Strength, ISO 604
  • Compressive Strength, ISO 604
  • K Factor (ISO)
  • Charpy Impact Unnotched, ISO 179-1/1eU
  • Charpy Impact, Notched, ISO 179-1/1eA, Partial Break
  • Coefficient of Friction, Dynamic
  • Volume Resistivity, IEC 60093
  • Surface Resistivity per Square, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Strength
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • CTE, linear
  • Thermal Conductivity
  • Melting Point, ISO 11357-1/-3, DSC, 10°C/min.
  • Maximum Service Temperature, Air, Continuous
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Flammability, UL94
  • Oxygen Index, ISO 4589-1/-2
  • 3A-Dairy
  • European Food 1935/2004
  • FDA
  • USP Class VI
  • Acids, Strong (pH 1-3)
  • Acids, Weak
  • Alcohols
  • Alkalies, Strong (pH 11-14)
  • Alkalies, Weak
  • Chlorinated Solvents
  • Continuous Sunlight
  • Hot Water / Steam
  • Hydrocarbons - Aliphatic
  • Hydrocarbons - Aromatic
  • Inorganic Salt Solutions
  • Ketones, Esters
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.