  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Alcohol (EVOH)

Material Notes: 32 mol % Ethylene. Non oriented type film; property values for 15 µm film.

Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier properties.

EVAL™ is now produced as a part of the Kuraray product line.

Key Words: Ethylene Vinylalcohol
Vendors:
Available Properties
  • Moisture Absorption at Equilibrium, 65% RH
  • Moisture Absorption at Equilibrium, 65% RH
  • Moisture Absorption at Equilibrium, 100% RH
  • Moisture Vapor Transmission, 40°C, 90% RH
  • Oxygen Transmission, 20°C; 65% RH; Permeability increases significantly at higher moisture content.
  • Thickness
  • Film Elongation at Break, MD, ASTM D638, 10%/min.
  • Film Elongation at Break, TD, ASTM D638, 10%/min.
  • Secant Modulus, MD, Youngs Modulus, ASTM D638, 10%/min.
  • Secant Modulus, TD, Youngs Modulus, ASTM D638, 10%/min.
  • Elmendorf Tear Strength MD, ASTM D638
  • Elmendorf Tear Strength TD, ASTM D638
  • Elmendorf Tear Strength, MD, ASTM D638, 0.6 mil
  • Elmendorf Tear Strength, TD, ASTM D638, 0.6 mil
  • Film Tensile Strength at Break, MD, ASTM D638, 10%/min.
  • Film Tensile Strength at Break, TD, ASTM D638, 10%/min.
  • Electrical Resistivity
  • Surface Resistance
  • Dielectric Constant, Frequency Not Specified
  • Dissipation Factor, Frequency Not Specified
  • CTE, linear, Estimated by MatWeb from similar grades
  • CTE, linear, Estimated by MatWeb from similar grades
  • Specific Heat Capacity, Estimated by MatWeb from similar grades
  • Thermal Conductivity, For EVAL F101
  • Melting Point, DSC
  • Haze, 65% RH
  • Gloss, 65% RH
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.