Availability: Asia Pacific; Europe; North America Fillers/Reinforcement: Glass Fiber, 28% Filler by Weight Additive: Impact Modifier Features: Creep Resistant; Good Stiffness; Good Toughness; Impact Modified Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |